Electrolytic Nickel Plating
| According to standard: | instruction MgG 10/78 |
|---|---|
| Corrosion resistance: | ASTM B117 |
| Nikl: | 10 - 15 µm; 24 - 100 h |
| Single layer thickness: | 10 - 15 µm |
| Max coating thickness: | 25 µm |
| Bath volume: | 780 dm3 |
| Batch size: | 210 dm2 |
| Color: | shiny silver |
| De-hydrogenation: | 150 - 200C° |
Electroless Nickel Plating
| According to standard: | instruction MgG 01/18 |
|---|---|
| Corrosion resistance: | ASTM B117 |
| Single layer thickness: | 10 - 15 µm uniform thickness |
| Max coating thickness: | 25 µm uniform thickness |
| Bath volume: | 300 dm3 |
| Batch size: | 94 dm2 |
| Color: | shiny silver |
| De-hydrogenation: | 150 - 200C° |